5.1 特性 Features
u 低寄生电容 Low stray Capacitance
u 氮化钽薄膜,形成自钝化保护膜 Tantalum nitride thin film , self – passivating
u 适合金丝键合 Fit to gold wire bonding
u 电极耐温特性400℃×6min Baking:400℃×6min
5.2运用 Applications
u 微波集成电路模块 Microwave integrated circuit module
u 光通讯 Optical communication
5.3 电阻器结构 Figuration
5.4产品编号 Part Number Code
产品代码 | 尺寸 | 材质 | 厚度 | 外形 | 电阻值 | 精度 | 镀层体系 | 包装方式 |
HR:薄膜电阻 | 0402 0603 0805 | A:99.6%Al2O3 D:96%Al2O3 N:AlN | 05 10 15 | A B C | 1R0:1.0Ω 100:10Ω 101:100Ω | J K M | T:TaN/TiW/Au F:TaN/TiW/Ni/Au | L:蓝膜 T:盒装 |
5.5选型指导 Selection Guide
★ TABLE5-1 选型推荐 Type Selection Recommendation
尺寸代码 | 0201 | 0402 | 0603 | 0805 | 1206 |
尺寸(mm) | 0.508×0.254(±0.05) | 1.016×0.508(±0.05) | 1.524×0.635(±0.05) | 2.032×1.27(±0.1) | 3.048×1.524(±0.1) |
阻值(Ω) | 推荐规格型号 | ||||
25 | HR0201A10N250KTT | HR0402A10A250KTT | HR0603A10A250KTT | ||
50 | HR0201A10N500KTT | HR0402A10A500KTT | HR0603A10A500KTT | HR0805A10A500KTT | |
75 | HR0201A10N750KTT | HR0402A10A750KTT | HR0603A10A750KTT | HR0805A10A750KTT | |
100 | HR0201A10N101KTT | HR0402A10A101KTT | HR0603A10A101KTT | HR0805A10A101KTT | HR1206A10A101KTT |
150 | HR0402A10A151KTT | HR0603A10A151KTT | HR0805A10A151KTT | HR1206A10A151KTT | |
200 | HR0402A10A201KTT | HR0603A10A201KTT | HR0805A10A201KTT | HR1206A10A201KTT | |
250 | HR0402A10A251KTT | HR0603A10A251KTT | HR0805A10A251KTT | HR1206A10A251KTT | |
500 | HR0805A10A501KTT | HR1206A10A501KTT | |||
1000 | HR0805A10A102KTT | HR1206A10A102KTT | |||
极限阻值(Ω) | 10~200 | 10~500 | 10~1000 | 10~1500 | 10~2000 |
注:1、如果产品使用时功率较大,应选用氮化铝做为基材;
2、可根据客户需求定制产品尺寸及阻值。
04-28
How to reflow Guangdong LED chip lamp bead
Now plug-in lamp beads and chip lamp beads are required to be reflow welded, so the lamp beads can basically be under 240 ℃.If the LED lamp bead is reflow welded, the reflow temperature must be set, o
04-28
How to deal with the leakage of high voltage chip lamp beads
1. The primer is too thick, which leads to leakage.2. For example, when the lamp bead is welded, the improper operation of the wire welding machine causes the excessive pressure when the magnetic nozz